top of page

S355J2

Steel Data Sheet

Chemical Composition (%)
EN 10025-2 (DIN 17100)

Mechanical Properties
Heat Treatment Status of the Sample: +AR

Comparison of International Steel Grades

S355J2 Çeliğinin S355Jr çeliğinden farkı çentik darbe testi uygulanmış olmasıdır. S355J2 Çeliğinin -20ºС sıcaklıkta darbe dayanımı en az 27 (KV) joule'dur.

Keywords: Keywords: 1.0037, What is 1.0037, 1.0037 Steel, 1.0037 Steel Properties, Material No: 1.0037, Material No: 1.0037, Wr. No: 1.0037, 1.0037 Material

Disclaimer

This page has been prepared in good faith for informational purposes only.

The accuracy, completeness and up-to-dateness of the information is not guaranteed or undertaken by Kanat Çelik Sanayi ve Ticaret A.Ş.

bottom of page